N17543
Douglas DC-9-32 FAA →
earlier registrations
1 past record
service difficulty reports
17 reports
- 14 Apr 1998
Beam, cracked
INSPECTION FOUND A 4 CRACK IN R-1 DOOR INTERIOR FORWARD NR 2 BEAM. THE CRACK WAS STOP DRILLED IAW SRM 52-05, FIGURE 25. A J-ANGLE, FITTING, AND SHIMS WERE…
- 4 Feb 1998
Coalescer Bags, dirty
SMOKE APPEARED IN THE CABIN AND COCKPIT AFTER TAKEOFF WITH THE ENGINE AND AIRFOIL ANTI-ICE ON. ALSO, THE RT AIR CONDITIONING SUPPLY TEMP HIGH LIGHT…
- 6 Oct 1997
Brake Rotor, broken
THE LT MLG BRAKE BEGAN TO DRAG DURING TAXI TO GATE IN TUL. THE FUSE PLUG BLEW AND THE LEFT TIRE (LEFT OUTBOARD MAIN) DEFLATED. MAINTENANCE FOUND THE LEFT…
- 11 Sep 1997
Duct, ruptured
THE NR 1 ENG POWER LEVER WAS DIFFICULT TO RETARD AFTER TAKEOFF FROM CLE. THE NR 1 ENG FIRE WARNING ACTIVATED 30 SECONDS AFTER SETTING CLIMB POWER. THE FIRE…
- 2 Mar 1997
Angle, cracked
INSPECTION FOUND LT SIDE STA 756 FAIRING ATTACH SUPPORT ANGLE CRACKED IN TWO PLACES. THE CRACKS WERE .25 AND 3 INCH LENGTH. THE SUPPORT ANGLE WAS REMOVED AND…
- 28 Feb 1997
Bracket, cracked
INSPECTION FOUND A 1 INCH CRACK IN SUPPORT BRACKET OF NR 2 ENGINE PYLON LEADING EDGE. A NEW BRACKET WAS FABRICATED AND INSTALLED IAW SRM 54-04, 51-30-2, AND…
- 28 Feb 1997
Channel, corroded
INSPECTION FOUND J-CHANNELS CORRODED AT STA 200, BL 0 TO RBL 20 AND RBL 24 TO 43 THE CHANNELS WERE REMOVED. NEW, CHANNELS WERE FABRICATED INSTALLED IAW SRM…
- 28 Feb 1997
Channel, corroded
INSPECTION FOUND J-CHANNELS CORRODED AT STA 160 TO 237, BL 0 AND STA 160, BL 0 TO LBL 60. THE CHANNELS WERE REMOVED, NEW CHANNELS WERE FABRICATED AND…
- 28 Feb 1997
Splice, corroded
INSPECTION FOUND STRINGER SPLICE PLATE CORRODED IN AFT PIT AT FS 965, STRINGER 29R. A REPAIR SPLICE WAS FABRICATED AND INSTALLED IAW SRM 51-10-2, 51-10-3, AND…
- 27 Feb 1997
Fillet, cracked
INSPECTION FOUND A 1 INCH CRACK IN LT WING FILLET PANEL. A REPAIR WAS FABRICATED AND INSTALLED IAW SRM 53-51-0.
- 27 Feb 1997
Subfloor, corroded
INSPECTION FOUND SUBFLOOR CORRODED AT STA 852, LBL 44. THE CORRODED AREA WAS REMOVED AND A REPAIR WEB WAS INSTALLED IAW SRM 53-01.
- 27 Feb 1997
Intercostal, corroded
INSPECTION FOUND INTERCOSTAL CORRODED BETWEEN STA 699 AND 718 AT LONGERON 16L. THE INTERCOSTAL WAS REMOVED AND A NEW INTERCOSTAL WAS FABRICATED AND INSTALLED…
- 25 Feb 1997
Subfloor, corroded
INSPECTION FOUND SUBFLOOR CORRODED AT FS 237, LBL 20 TO 44. THE CORRODED AREA WAS REMOVED, A REPAIR WAS FABRICATED AND INSTALLED IAW SRM 53-11-2 AND 53-01,…
- 19 Feb 1997
Doubler, corroded
INSPECTION FOUND DOUBLER CORRODED AT STA 897. THE DOUBLER WAS REMOVED AND A REPLACEMENT WAS FABRICATED AND INSTALLED IAW SRM 53-11-3 AND 51-30-2.
- 13 Apr 1996
Strut, flat
GSO - FLT 1147 - THE LANDING GEAR WOULD NOT RETRACT AFTER TAKEOFF FROM GSO. 'ABNORMAL' PROCEDURES WERE C/W, BUT, THE GEAR HANDLE WOULD ONLY GO TO THE UPLATCH…
- 12 Apr 1996
Tab, delaminated
GSO - INSPECTION FOUND A 2 SQUARE INCH AREA OF RUDDER TAB LEADING EDGE DELAMINATED. THE AREA WAS REPAIRED USING BONDED DOUBLER AND FILLER. A WEIGHT AND…
- 10 Apr 1996
Skin, cracked
GSO - INSPECTION FOUND A 4 INCH BY 2 INCH HOLE AND SEVERAL CRACKS TOTALING 12 INCHES IN LENGTH IN SKIN PANEL ABOVE RUDDER ON RIGHT SIDE OF VERTICAL…